Time: 2026-11-04 12:55:46
Click:
Lithium battery manufacturing involves several processes in which conductive metal components must be connected reliably.
These components may include aluminum electrode tabs, copper electrode tabs, multilayer metal foils, terminal connections, and conductive parts used in battery modules.

For selected applications, ultrasonic metal welding offers an alternative to conventional fusion welding and mechanical joining.
The process uses high-frequency mechanical vibration combined with controlled pressure to create a solid-state metal bond. Rather than relying on melting the base metals, the relative movement at the contact interface helps disrupt surface films and establish intimate contact between the materials.
This makes ultrasonic metal welding particularly relevant to applications involving thin conductive materials and stacked metal layers.
However, it is important to understand that not every connection in a lithium battery is made using the same welding process. The appropriate joining method depends on the battery design, connection location, material combination, and production requirements.


Battery electrodes contain conductive current collectors, commonly based on aluminum and copper. Their electrical connection to the corresponding tabs is an important part of the cell assembly process.
Ultrasonic metal welding can be used in suitable designs to join compatible tab materials and stacked conductive foils.
Typical materials include:
The actual material combination depends on the battery chemistry, electrode structure, and cell design.
In some battery designs, multiple thin metal foils need to be joined together.
The number of layers affects the total stack thickness and the way vibration and pressure are transmitted through the joint.
A process suitable for a small number of foil layers may not work properly with a thicker stack.
Manufacturers should therefore evaluate the actual material thickness, layer count, tab width, and required weld area before selecting the machine and tooling.

Multilayer foil welding presents specific process challenges.
If the welding energy or pressure is unsuitable, the material may experience excessive deformation, tearing, inconsistent bonding, or other defects.
Several factors should be considered:
Material properties
Aluminum and copper have different mechanical and physical properties. Their response to ultrasonic vibration and pressure is not identical.
Total stack thickness
The combined thickness of the foil layers influences the required welding conditions.
Welding area
The width, length, and geometry of the intended joint determine the tooling contact requirements.
Sonotrode surface design
The working surface of the sonotrode influences how vibration and pressure are transferred to the foil stack.
Process parameters
Amplitude, pressure, welding time, and energy settings must be evaluated together.
For this reason, manufacturers should validate the process using representative material samples rather than relying only on nominal machine power.
At this stage, conductive components may need to be connected to form series or parallel electrical arrangements.
Depending on the battery architecture, these connections may involve:
It is important to distinguish these applications from electrode tab-to-foil welding inside a cell.
Battery pack connections often involve different material thicknesses, joint dimensions, fixture arrangements, and mechanical requirements.
For thicker busbars or larger connecting components, other joining technologies may also be appropriate. The choice should be based on the actual connection design and process validation.

The following factors deserve particular attention.
Copper-to-copper, aluminum-to-aluminum, and compatible dissimilar-metal combinations have different process characteristics.
Material grade, surface condition, thickness, and contamination should all be considered.
Pressure helps maintain contact between the workpieces during ultrasonic vibration.
Insufficient or excessive pressure may affect joint formation, material deformation, and process consistency.
Amplitude influences the relative movement at the metal interface.
The suitable amplitude depends on the material combination, thickness, layer count, tooling, and required weld area.
Welding time and energy are important process-control variables.
Too little energy may result in inadequate bonding. Excessive energy may cause material damage or undesirable deformation.
A suitable process window should be established through sample trials and quality testing.
The sonotrode transfers ultrasonic vibration to the workpiece, while the fixture and anvil support the materials during welding.
Their geometry, contact surfaces, alignment, and mechanical condition can influence the repeatability of the welding process.
A tooling design developed for one battery tab configuration should not automatically be used for a different product.
The following information is useful for an initial technical evaluation:
| Material | Copper, aluminum, nickel, or material combination |
| Material thickness | Thickness of each layer and total stack |
| Layer count | Number of foils or metal layers |
| Tab dimensions | Width, length, and thickness |
| Weld area | Required joint dimensions |
| Connection type | Foil-to-tab, tab-to-terminal, or module connection |
| Production target | Required cycle time and output |
| Quality criteria | Mechanical and electrical requirements |
Representative samples are especially important.
A machine that performs well on one material combination may require different tooling or process parameters for another.
Before mass production, manufacturers should establish appropriate inspection procedures, which may include visual examination, peel or pull testing, cross-section analysis, and electrical resistance measurement.
The acceptance criteria should be defined according to the battery manufacturer's product specifications and quality requirements.
Important equipment specifications include:
For example, Qijiang Precision's JS-2040 ultrasonic metal welding system is designed for industrial metal-joining applications, including suitable battery tab and conductive metal component welding.
The system uses a 20 kHz ultrasonic frequency and a 4000 W rated power configuration. Its application suitability depends on the material, total thickness, joint dimensions, tooling, and validated process conditions.
The final machine configuration should be confirmed through application testing.
Ultrasonic metal welding has several potential applications in lithium battery manufacturing, including electrode tab connections, multilayer foil joining, and selected battery module interconnections.
However, these applications do not share one universal welding specification.
Material combination, foil layer count, joint geometry, pressure, amplitude, energy input, and tooling all influence the result.
For battery manufacturers, the most reliable approach is to evaluate the actual workpiece, validate the welding process, and select equipment according to the production requirements.
About Qijiang Precision
Wuxi Qijiang Precision Machinery Co., Ltd. specializes in ultrasonic metal welding equipment and customized ultrasonic joining solutions for industrial manufacturing.
We support application evaluation for copper and aluminum metal joining, battery tab welding, and other conductive component connections.
To discuss your battery welding application, please share your material specifications, workpiece drawings, and representative samples.
Contact Qijiang Precision for an ultrasonic metal welding application evaluation.